Dell 2355dn All in One Printer User Manual


 
315
Paper Specifications
Paper Output Capacity
Printer and Paper Storage Environment
Paper storage environmental conditions directly affect the feed operation.
Ideally, the printer and paper storage environment should be at or near room temperature, and
not too dry or humid. Remember that paper is hygroscopic; it absorbs and loses moisture
rapidly.
Heat works with humidity to damage paper. Heat causes the moisture in paper to evaporate,
while cold causes it to condense on the sheets. Heating systems and air conditioners remove
most of the humidity from a room. As paper is opened and used, it loses moisture, causing
streaks and smudging. Humid weather or water coolers can cause the humidity to increase in a
room. As paper is opened and used it absorbs any excess moisture, causing light print and
dropouts. Also, as paper loses and gains moisture it can become distorted. This can cause paper
jams.
Care should be taken not to purchase more paper than can be used in a short time (about 3
months). Paper stored for long periods may experience heat and moisture extremes, which can
cause damage. Planning is important to prevent damage to large supplies of paper.
Category Specifications
Acid Content 5.5 pH or lower
Caliper 0.094-0.18 mm (3.0-7.0 mils)
Curl in Ream Flat within 0.02 in. (5 mm)
Cut Edge Conditions Cut with sharp blades with no visible fray.
Fusing Compatibility Must not scorch, melt, offset or release hazardous emissions when
heated to 180° C (356° F) for 0.1 second.
Grain Long Grain
Moisture Content 4%-6% by weight
Smoothness 100-400 Sheffield
Output Location Capacity
output tray (Face Down) 150 sheets of 75 g/m
2
bond (20 lb) paper
rear door (Face Up) 1 sheet of 75 g/m
2
bond (20 lb) paper